1. Heat treatment

PSL1 requirements: J55 and K55 same way (can be rolled-state delivery);

PSL2 requirements: J55, K55 product should be normalized or normalized and tempered overall, if thick, should be normalized or normalized and tempered after thickened.

 

2. Tensile test

J55: yield strength of 379MPa ~ 552MPa; tensile ≥517MPa; minimum elongation of J55 is 19%.

K55: yield strength of 379MPa ~ 552MPa; tensile ≥655MPa; minimum elongation of K55 is 15%.

 

3. Impact test

J55 and K55 impact test must be done, the minimum size of the sample lateral impact energy 20J, the smallest full-size sample longitudinal impact energy 27J.

 

4. Wall thickness detection

PSL1: J55 and K55 for measuring the wall thickness of no coverage requirements;

PSL2: J55 and K55 for wall thickness measurement and recording deal with the entire length of the best coverage of the surface area of automatic detection system should reach 25%.

 

5. NDT

PSL1: J55 and K55 on the tube did not do destructive testing mandatory requirements;

PSL2: J55 and K55 for all pipe shall be one or more of the criteria specified in 10.15.5 tested to find the inner surface of the outer surface of the pipe and can receive the level of L4 longitudinal imperfections.


HOT PRODUCT

QUICK LINKS

CONTACT US

  Hunan Gaoxing Steel Development Zone, No.1888 Purui South Rd, Wangcheng District,Changsha, Hunan, China

Tel: 0086-0731-88739521

  inquiry@threewaysteel.com

Copyright  2020 Threeway Steel Co.,Ltd. All Rights Reserved
PRODUCT INQUIRY